Stress corrosion testing machine
Stress corrosion testing machine

Home page >> Product display >> Stress corrosion testing machine >> Ultrapure water medium slow strain rate stress corrosion testing machine

Ultrapure water medium slow strain rate stress corrosion testing machine
Ultrapure water medium slow strain rate stress corrosion testing machine

Ultrapure water medium slow strain rate stress corrosion testing machine

This equipment is used to test the corrosion resistance of materials in ultrapure water medium environment.The equipment consists of a load-bearing frame, a loading unit, a control system, an experimental kettle, a heating system, a DCPD crack growth measurement system, and test software.The experim

  • Stress corrosion testing machine | Release time:2026-07-29 18:13:20

Equipment brief description:

This equipment is used to test the corrosion resistance of materials in ultrapure water medium environment.

The equipment consists of a load-bearing frame, a loading unit, a control system, an experimental kettle, a heating system, a DCPD crack growth measurement system, and test software.

The experimental kettle and high-temperature furnace can be lifted and lowered electrically to facilitate the installation of specimens.The system is a static corrosive medium environment. After the ultrapure water is injected into the experimental kettle, the valve is closed, and the corrosive medium is sealed in the kettle.The heating is turned on, and the thermostat keeps the temperature constant after reaching the set temperature.Heating generates thermal expansion pressure, and the pressure balance device eliminates the additional attachment force exerted on the specimen by the pressure in the kettle.The lid of the experimental kettle has interfaces for water injection, drainage, temperature measurement, DCPD measurement, reference electrode, etc.

The DCPD system realizes crack preset, fatigue crack measurement, corrosion crack measurement, constant K test, rising K test, falling K test, and crack expansion rate measurement of CT specimens in corrosive medium environment.

Experimental features:

Ordinary tensile test.

Constant load creep/stress corrosion testing.

Slow strain rate tensile testing.

Low cycle fatigue/corrosion fatigue testing.

Test for measuring crack initiation and crack propagation rate of specimens.

Constant K control, rising K control, and falling K control tests.

Features:

Dynamic display: Load, displacement, deformation, time and test curves are dynamically displayed on the screen in real time.

Record and output stress-strain, force-time, force-displacement and other test data and curves.

Supports long-term continuous testing.

The test control is streamlined and the test process conditions can be compiled by oneself.

Automatic protection: Automatic protection and memory when force value reaches, time limit, breakage, etc. occur.

Automatic data processing: The test software automatically processes data according to corresponding standards.

Data is saved at any time and retained when power is turned off.

The test results can be stored and can be read and consulted at any time.

Test data and curves can be reanalyzed, and curves can be enlarged arbitrarily.

The open test report supports customized report templates, automatically generates test reports, can be printed or previewed, and can be saved as a file.

It has software limit protection, stroke limit protection, and full-scale overload protection functions.

Equipment features:

High rigidity heavy load frame.

High-performance fully digital servo loading control system with high speed control accuracy.

Using grating displacement sensor, the sample deformation measurement accuracy is high.

Integrated measurement and control system facilitates expansion and use.

Realize crack growth measurement in corrosive media environment.

Technical indicators:

Product modelHYMYL-50
Maximum test force50kN
Test force measurement range1%~100%F.S.
Test force indication accuracy±0.5%
Test force resolution±180000 codes, no binning throughout, resolution remains unchanged
Loading head movement range80mm
Loading head movement speed10mm/s~1x10-6mm/s
Loading head displacement indication accuracy±0.5%
Loading head displacement resolution0.05µm
Deformation measurement range0~30mm
Deformation indication accuracy±0.5%
Deformation resolution0.001mm
Fatigue loading waveformSine wave, triangle wave
Fatigue loading frequency0.0001~1Hz
Crack measurement length resolution1µm
Heating furnace temperature range<500℃
Experimental kettle working temperature≤350℃
Maximum work pressure20MPa
Quickly Quotation

WeChat scan code consultation

400-6656-17718866878767