Home page >> Product display >> Stress corrosion testing machine >> Constant load corrosion bending testing machine
1. Equipment name: Constant load corrosion bending testing machine
2. Equipment introduction: The constant load corrosion bending testing machine is used to conduct corrosion bending tests on FRP materials in corrosive environments.The host structure is in the form of four columns, and the loading mode uses a servo motor loading unit for loading.This test system consists of a bending loading system, a corrosive environment container, a heating system, a test fixture, a measurement and control system, a test software, a computer, and a control cabinet.
3. Technical parameters:
1) Maximum test force of loading spindle: 10kN
2) Number of loading spindles: 2 axes in total; can be loaded independently without interfering with each other;
3) Test force range: 1%~100%F.S.
4) Relative error of test force indication: ±0.5%
5) Relative error of test force constant load: ±0.5%
6) Maximum moving range of loading head: 80mm
7) Loading head moving speed: 2.5mm/s~1x10-7mm/s
8) Loading head displacement measurement accuracy: ±0.5%
9) Loading head displacement resolution: 0.0125µm
10) Deformation measurement range: 0~40mm
11) Deformation measurement resolution: 1µm
12) Deformation measurement accuracy: ±0.5%
13) Working environment: NaOH, acidic substances;
14) Working temperature: normal temperature ~ 120℃;
15) Environmental pressure: normal pressure;
16) The experimental kettle adopts electric heating, and the temperature system control accuracy is ±1°C.
17) Temperature measurement: S-type thermocouple.